Dark and pale fabric swatches arranged for apparel quality assessment

Colour Fastness: How to Read Textile Test Reports

Colour fastness is a textile’s resistance to changes in colour and to transferring colour under specified conditions. A fabric can retain its appearance during washing yet transfer colour when rubbed wet. It can also stain another material without an equally obvious change in its own shade.

That is why “colour fastness: 4” is not enough information for a clothing purchase. You need the test, conditions, specimen, evaluation and scale behind the number. This guide explains how to read those details for South African and international apparel orders. Color fastness, the American spelling, describes the same concept—not a different property.

Two Outcomes: Colour Change and Staining

Colour change concerns the original textile: how its appearance differs after the specified exposure compared with an unexposed reference. A change can involve shade or depth, not just obvious fading.

Staining concerns another material receiving transferred colour, such as an adjacent test fabric or a rubbing cloth. In tests using multifibre adjacent fabric, the report may show separate staining results for its different fibre components. Do not replace those readings with the most favourable value.

ISO treats these as distinct evaluations: ISO 105-A02:1993 describes the grey scale for colour change; ISO 105-A03:2019 covers staining. These are assessment tools, not universal purchasing specifications.

Pairs of coloured swatches and white cloth pieces illustrating colour change and transferred colour

AI-generated conceptual illustration, not tested specimens or a calibrated grading reference.

A dark shirt beside a white collar illustrates why both outcomes matter. Preserving the shirt’s shade does not establish that the collar will remain unstained. Conversely, a staining result does not describe every possible change in the shirt itself.

Read the Rating Scale Before the Grade

Grey scales: commonly 1–5, with half-grades

The colour-change and staining grey scales commonly run from 5 to 1, with half-grades such as 4-5 and 3-4. Five represents no assessed difference at that scale’s top reference; lower grades represent progressively greater difference or staining. Grade 1 is the lowest reference, not necessarily complete loss of colour.

SDC Enterprises’ grey-scale description lists the nine steps in the augmented scales. A notation such as 3-4 is an intermediate grade, not “three out of four” or an interval of uncertain test results. A staining grade and a colour-change grade still describe different objects, even when their numbers match.

Read whether assessment was visual or instrumental and which procedure was used. A photograph on a phone is not a calibrated grey scale; lighting, background and display settings can change what you see.

Blue wool: a lightfastness reference system

The commonly used blue wool series 1–8 ranks reference materials from lower to higher resistance to light. SDC’s blue wool explanation describes this progression. An 8 is not a promise that a garment will never fade.

ISO 105-B02:2014 addresses artificial daylight using a xenon-arc source. Its public scope allows two blue wool reference sets and warns that their results may differ. Identify the reference system, exposure method and endpoint; do not assume every lightfastness report uses one interchangeable 1–8 scale.

Grey-scale assessment can also be involved in evaluating fading during a light test. Therefore, ask whether a reported number is a blue wool comparison or colour change after a stated exposure. A lightfastness 4 is not equivalent to a washing grey-scale 4, and neither number converts directly into years of outdoor wear.

What the Main Colour Fastness Tests Actually Cover

Washing exposes specimens to a defined laundering procedure. Rubbing, also called crocking, examines colour rubbed off onto another material. Light testing examines colour response to controlled light exposure. Perspiration tests use specified simulated sweat conditions; water testing addresses immersion under its own conditions.

Intertek’s testing overview links these exposures to different garment risks. None substitutes for all the others. A wash result does not cover sunlight, and a dry-rubbing result does not establish wet-rubbing behaviour.

The matrix below is a reading framework, not a completed test report. Record the actual specimen or material, conditions, separate results and scale from your supplier’s document. Unknown means evidence has not been established; not applicable should be used only when the evaluation genuinely does not belong to that test.

Colour Fastness Test Report Reading & Application Matching Matrix

On a small screen, scroll the matrix horizontally to read every column.

Test purpose → applicable method Specimen, conditions → separate results and scale Intended garment use → buyer interpretation and evidence gaps
Laundering: ISO 105-C06:2010 Identify fabric, colour and batch; record procedure, detergent/bleach, temperature, time and mechanical action. Keep colour change and each adjacent-fabric staining grade separately; identify assessment scale. Missing details: Unknown. Everyday clothing, school uniforms and frequently washed apparel: match the tested procedure to documented care and purchasing requirements. An ordinary laundering result does not establish industrial-laundry suitability.
Rubbing: ISO 105-X12:2016 Identify specimen face/direction and rubbing cloth; retain dry/wet conditions and preparation details. Record staining on the rubbing cloth separately for dry and wet tests, with the assessment scale. Specimen colour change is not the primary endpoint. Dark garments and contact-prone workwear: assess transfer risk independently of shade retention. Missing wet evidence remains Unknown even when a dry grade is available.
Light: ISO 105-B02:2014 Identify colour/component, exposure method, reference set, conditions and endpoint or dose. Record the reported lightfastness comparison or colour-change assessment with its scale. Adjacent-fabric staining is not the normal endpoint. Outdoor clothing: check whether exposure and acceptance requirements address the intended use. Missing reference set or exposure details prevents straightforward comparison; the result is not a service-life forecast.
Perspiration: ISO 105-E04:2013 Identify specimen and adjacent fabrics; retain acid/alkaline results, treatment conditions, pressure, temperature and duration. Record colour change and staining separately with their assessment scales. Missing items: Unknown. Sportswear, uniforms and other skin-contact clothing: examine both shade change and transfer to other components. Sweat evidence alone does not establish wet-rubbing or wash performance.
Water: ISO 105-E01:2013 Identify specimen and adjacent fabrics; retain immersion and subsequent treatment conditions. Record colour change and staining separately, with their scales. Missing results: Unknown. Clothing subject to wet contact: compare the water exposure with the purchasing brief. Do not infer detergent-wash, seawater, chlorinated-water or waterproof performance from this result.

Method scopes: ISO C06, X12, B02, E04 and E01. The matrix lists report-reading questions; it is not a laboratory operating procedure.

ISO and AATCC names are not automatic equivalents

AATCC’s official catalogue includes TM8 for crocking, TM61 for accelerated laundering, TM15 for perspiration and TM16.3 for xenon-arc light testing. Use the full designation and edition written on the report, including the selected option where relevant.

For example, AATCC TM15-2021e evaluates acid perspiration. ISO 105-E04:2013 uses acid and alkaline solutions. A shared “perspiration” heading therefore does not establish identical coverage. Likewise, AATCC TM61 describes accelerated laundering; do not turn its result into an unconditional guarantee for a fixed number of home washes.

Match Evidence to the Actual Garment

Start with exposure, not a supposedly superior fibre. Dye selection, processing, finishing and the tested construction matter alongside composition. Our polyester vs cotton guide explains why a fibre name alone cannot determine garment performance.

  • Everyday clothing: prioritise the planned wash routine and likely transfer to other clothes or surfaces.
  • School uniforms: consider frequent laundering, repeated colour matching and contrast components such as pale collars.
  • Workwear: define whether care is domestic or a specialist laundry process; do not assume the same report covers both.
  • Sportswear: consider perspiration, wet contact, friction and laundering as separate questions.
  • Dark-coloured garments: look closely at dry and wet rubbing results, particularly where the cloth contacts light materials.
  • Outdoor clothing: include relevant light evidence alongside washing and moisture exposures; lightfastness does not establish weatherproofing.

School shirt, work shirt and sports top arranged to compare clothing use contexts

AI-generated apparel-use illustration; no performance ranking is implied.

Verify that the report represents the actual colour, finish and supplied material. A result for one dye lot or colourway is not automatic evidence for all alternatives. For patterned materials, ask which colours and components were tested; our jacquard fabric guide explains why the construction name alone leaves composition and specifications unresolved.

Keep four layers separate: test method describes the assessment; reported result describes the tested specimen; buyer acceptance criteria define the agreed requirement; product suitability also depends on the intended garment and use. There is no single global “grade 4 passes everything” rule.

Hypothetical Supplier Test Report Interpretation Example

Entirely hypothetical: a buyer considers navy cotton-polyester fabric for school shorts worn with pale shirts. No supplier, laboratory, certificate or real test is represented here.

The imagined report identifies the finished fabric, navy colour, batch and sample date. It names ISO 105-X12:2016 and records specimen direction, rubbing cloth, preparation, apparatus conditions and separate dry/wet testing. Its reported endpoint is rubbing-cloth staining on the stated grey scale: dry 4; wet 3. It does not report a specimen colour-change grade for rubbing.

The imagined purchase specification requires dry staining of at least 4 and wet staining of at least 3-4, using that same method and agreed conditions. These thresholds are invented solely for this example—not ISO requirements or South African market minimums.

Interpretation: dry meets this particular requirement; wet does not. Do not average them into a passing number. Resolve the wet-transfer concern with the supplier before approval, potentially through process changes and retesting of representative material.

Washing, perspiration and light results are Unknown because this imagined report contains none. That does not mean the fabric failed those tests. Determine which are relevant to the shorts, then request the missing evidence. If the specimen identity or wet-test conditions were absent, even the initial comparison would need clarification before relying on it.

A Seven-Step Purchasing Check

  1. Identify intended use: garment, contact materials, wearing environment and care routine.
  2. Select relevant tests: connect each exposure to a question the test can answer.
  3. Verify conditions: method edition, option, specimen identity, pretreatment and exposure details; record deviations.
  4. Separate results: colour change, staining by adjacent fibre, dry/wet rubbing and the stated light reference system.
  5. Compare documented requirements: apply the buyer’s agreed limits only to comparable methods and conditions.
  6. Identify missing evidence: mark Unknown, assign a question and request clarification; do not silently turn a blank into a pass or failure.
  7. Decide on further testing: use relevance and uncertainty to choose clarification, representative testing or a revised material—not a blanket test list for every garment.

Retain the full report and its sample references rather than a cropped grade screenshot. For a material purchase, confirm composition, finish and care as well; the linen fabric buying guide shows how to separate verified specifications from a fabric’s marketing name.

What a Home Spot Check Can—and Cannot—Tell You

A discreet check following the garment’s care instructions may reveal visible transfer or colour loss. Treat that as a practical warning, not an ISO or AATCC grade. A check without controlled preparation, exposure, assessment materials and traceability does not provide equivalent evidence to the corresponding standard test.

No visible transfer in one check proves nothing about untested sunlight, repeated washing, sweat or another colourway. Avoid using a home check to justify aggressive washing or a guaranteed “colour-safe” claim. Ask for relevant evidence when the purchasing decision needs more than an informal screen.

The useful question is not “Is this fabric colourfast?” It is: colourfast to which exposure, under what conditions, assessed how, and sufficient for whose documented use? Read the report through that lens before approving the material.

Sources and Scope

Public source descriptions checked 19 October 2026. Use the applicable complete standard and agreed specification for testing and acceptance. This article reports no first-hand tests or product certification.